The color and pattern on stamped concrete sit at the surface under a film of sealer, so washing it is as much about the sealer as the dirt. Ace Concrete Construction pours stamped and colored slabs out of Taylors, and our page on stamped and decorative concrete in the Upstate covers the pour itself.
Below is how hard to wash and when a wash turns into a reseal, then the months of the year checked against the NOAA record from the weather station at Greenville-Spartanburg International Airport, which NOAA lists under Greer. Permits and county lines in town are on our page about concrete work in Greer. Part of Greer lies in Spartanburg County, where we also keep an office, listed on our page for a concrete contractor in Spartanburg, SC.
How much pressure can stamped concrete take?
Enough to get into the texture. The published figures for cleaning a stamped slab before it is sealed start at 3,000 psi.
Brickform's technical sheet for Gem-Seal 700 VOC, a solvent-based acrylic sealer it lists for stamped and colored concrete, says pressure washers used to clean slabs should run at a minimum of 3,000 psi at 4 gallons per minute. It adds that a rotary floor scrubber used on a stamped slab needs nylon bristle brush attachments, because pads do not reach the imprinted areas.
The Decorative Concrete Council of the American Society of Concrete Contractors (ASCC) sets the bar a little higher. Its best-practice sheet on sealing stamped concrete calls a power washer of at least 3,500 psi the most effective and efficient cleaning method, and for a reseal it recommends that pressure followed by 24 hours of drying time.
Both figures describe getting a slab ready for sealer, not a weekly rinse.